    The joint won't rust/corrode any more
    than your 1/4 plate. Use 309 wire.
    Brian Scott
    225LX
    Speedglass 9002v helmet
    19" Shop Fox band saw
    Ingersoll Rand air compressor

  2. #22

    Default

    Quote Originally Posted by brianscott View Post
    The joint won't rust/corrode any more
    than your 1/4 plate. Use 309 wire.
    Yeah, not worried about rust. I just want to get a good weld because this 1.5" Stainless bar will be supporting the loading arm for weights on the machine so I don't want the weld to fail!!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #23

    Default

    Recieved my Onlinemetals order yesterday and figured out that 1 1/2" Stainless round bar is Heavy!! I might need to use 1 1/2" Stainless tube for my application.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  4. #24
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,177

    Default

    Too heavy!?!? Remember you're doing this so you can be a weightlifter!!

    Kidding, of course. But here's one for the group: other posts have talked about the need to purge the inside of an SS tube weld. At what point does that become necessary? Is it only on very thin material where the opposite side of the weld glows red, or might CGCInc encounter that need even on heavier material?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  5. #25

    Default

    Quote Originally Posted by DaveO View Post
    Too heavy!?!? Remember you're doing this so you can be a weightlifter!!

    Kidding, of course. But here's one for the group: other posts have talked about the need to purge the inside of an SS tube weld. At what point does that become necessary? Is it only on very thin material where the opposite side of the weld glows red, or might CGCInc encounter that need even on heavier material?
    Good question! If I do use tubing it will be 1/4" wall

    I looked up the weight of round bar... around 6lbs. per foot.
    I will be using a 20" piece for the "curl" bar, a 2" x 6" piece of pipe with brass bushings in it that will slip over the 1 1/2" bar and some 1" tubing that will be welded to the 2" pipe for hand grips..... By the time it's all together, I'll be starting out lifting 50lbs.!!! Actually it will be around 14lbs.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  6. #26

    Default

    you dont have to back purge, but it is always recommended.. and thats only when your doing a butt weld to join the pipe. if your say putting a plate on the end and you do a fillet around the pipe, then you dont need any purging.
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  7. #27

    Default

    Although I don't have much experience welding stainless to mild steel, I have read many times that it's preferred to "butter" the mild steel with the 309 before making the actual weld. I believe this is to lower the amount of dilution of the filler metal with the mild steel.
    Maybe someone with more experience in this area can chime.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  8. #28

    Default

    Quote Originally Posted by CGCINC View Post
    Recieved my Onlinemetals order yesterday and figured out that 1 1/2" Stainless round bar is Heavy!! I might need to use 1 1/2" Stainless tube for my application.
    I have lots of 1.5 304 drops in .065 ( 16ga ) wall and lighter if you need a chunk
    Todd

  9. #29

    Default

    Quote Originally Posted by todmorg View Post
    I have lots of 1.5 304 drops in .065 ( 16ga ) wall and lighter if you need a chunk

    Well, I'm thinking I need 11ga. or thicker wall because this 18"-20" piece will be what I pull on to lift the weight and with it being that long, I don't want it to flex or bend. ( Any help is appreciated because I just don't know) I would say the most I will be lifting is 150lbs.

    Here is a diag. of what I'm doing. The 2" square tubing will be drilled all the way through so I can insert the 1.5" Stainless and weld on both sides of the square tubing.
    The center section(not gray) is a piece of 2" x 4" Rectangle tubing with a piece of 2" pipe on top. Another piece of the 1.5" Stainless will be running through the pipe and connecting both pieces of 2" Square tubing.
    Last edited by CGCINC; 12-27-2011 at 12:24 AM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •